Brand Name : High Broad
Model Number : 99.9 Scandium
Certification : ISO
Place of Origin : CHINA
MOQ : 100g
Price : TBA
Payment Terms : T/T, Western Union, L/C, D/A, D/P, T/T, MoneyGram
Packaging Details : Scandium in vacuum packaging
Supply Ability : 100kgs each year
Delivery Time : About 7 days
Material : Scandium
Purity : TREM 99-99.95%, Sc/TREM 99.9% min.
Crystal Structure : Hexagonal closed-packed
Chemical Formula : Sc
Application : 99.9 Scandium Metal Applied In Various Superalloys
High Purity Scandium Metal Applied In Various Superalloys
High Broad is able to supply scandium metal in purities from 99.5% to 99.999%, as well as scandium oxide (Sc2O3) in purities from 99.99% min. Please contact us with your specific requirement or for a current scandium price.
Scandium is a very light elemental metal that is often found alongside the rare earth elements. Due to it's rarity and high price, scandium does not have a lot of commercial applications, but is used in specialty halide lamps, as well as lightweight, high-strength alloys. It is estimated that only as little as a couple hundred kilograms of scandium metal are produced each year.
Chemical Formula: Sc
Description: Light, silvery-grey metal
Purity: TREM 99-99.95%, Sc/TREM 99.9% min.
Packing: As required
CAS No: 7440-20-2
| RE Element | Max. Impurity (ppm) | Element | Max Impurity (ppm) |
| La | 4.5 | Mn | 9.3 |
| Ce | 7.3 | Fe | 20.8 |
| Pr | 3.5 | Si | 10.2 |
| Nd | 6.9 | Ca | 9.9 |
| Sm | 4.3 | Mg | 1.3 |
| Eu | 1.9 | Cu | 9.4 |
| Gd | 8.3 | Ni | 5.7 |
| Tb | 4.4 | Al | 34.9 |
| Dy | 5.9 | Zn | 4.0 |
| Ho | 8.2 | Ti | 35.2 |
| Er | 5.5 | Ag | 1.6 |
| Tm | 6.3 | Cd | 0.8 |
| Yb | 2.0 | O | 280 |

|
|